Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.13 % Show Supplier Material materials with Moisture absorption of 0.13 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative Dichte of 1.2 [-] | ASTM D 792 | |
Specific volume | 23.0 °C | 0.85 cm³/g Show Supplier Material materials with Specific volume of 0.85 cm³/g | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.27 % Show Supplier Material materials with Wasserabsorption of 0.27 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 108 MPa Show Supplier Material materials with Biegefestigkeit of 108 MPa | ISO 178 | yield, 2 mm/min | ||
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | ISO 527 | yield, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527 | 1 mm/min | ||
Erichson scratch depth | 23.0 °C | 14 µm Show Supplier Material materials with Erichson scratch depth of 14 µm | SABIC method | 6N | ||
Hardness, Ball Indentation | 23.0 °C | 128 MPa Show Supplier Material materials with Hardness, Ball Indentation of 128 MPa | ISO 2039-1 | H358/30 | ||
Hardness, Pencil test | H | ASTM D 3363 | 1kgf | |||
Hardness, Rockwell L | 23.0 °C | 108 [-] Show Supplier Material materials with Hardness, Rockwell L of 108 [-] | ASTM D 785 | ||
Härte, Rockwell M | 23.0 °C | 93 [-] Show Supplier Material materials with Härte, Rockwell M of 93 [-] | ASTM D 785 | | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D 256 | notched, -30°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 30 J Show Supplier Material materials with Instrumented Impact, Total Energy of 30 J | ASTM D 3763 | 23°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 47 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 47 kJ/m² | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 4 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 45 kJ/m² | ISO 180/1U | unnotched 80*10*3, -30°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | SABIC method | CS-17, 1 kg | ||
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | ISO 527 | yield, 50 mm/min | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Ball pressure temperature | 140 °C Show Supplier Material materials with Ball pressure temperature of 140 °C | IEC 60695-10-2 | approximate maximum | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 131 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 118 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 118 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Spezifische Wärmekapazität | 23.0 °C | 1.4E-3 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 1.4E-3 J/(kg·K) | ASTM C 351 | ||
Vicat-Erweichungstemperatur | 138 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 138 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 118 - 131 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 118 - 131 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.2 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100081394- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥2.5mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Optisch
Property | Value | Comment |
---|---|---|
Brechungsindex | 1.58 [-] Show Supplier Material materials with Brechungsindex of 1.58 [-] | ISO 489 |
Opazität | 0.8 % Show Supplier Material materials with Opazität of 0.8 % | <, ASTM D 1003 | 2.54 mm |
Transmission | 88 % Show Supplier Material materials with Transmission of 88 % | ASTM D 1003 | 2.54 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 14.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 14.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 13 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 13 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Displays, Wiring Devices, Wireless Communications, Small Appliance | |
Availability | Europe,Asia,MEA,Americas,Global | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |