Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.34 [-] Show Supplier Material materials with Relative Dichte of 1.34 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 101 MPa Show Supplier Material materials with Biegefestigkeit of 101 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 5.3 GPa Show Supplier Material materials with Biegemodul of 5.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 4.2 % Show Supplier Material materials with Dehnung of 4.2 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 74 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 74 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 357 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 357 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, Total Energy of 16 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 74 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 74 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 74 MPa Show Supplier Material materials with Zugfestigkeit of 74 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 99 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 99 °C | ASTM D 648 | 6.4 mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 99 - 105 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 99 - 105 °C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=228536- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,MEA,Americas,Global | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |