Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.42 g/cm³ Show Supplier Material materials with Dichte of 1.42 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.42 [-] Show Supplier Material materials with Relative Dichte of 1.42 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 412 MPa Show Supplier Material materials with Biegefestigkeit of 412 MPa | ISO 178 |
Biegemodul | 23.0 °C | 25.4 GPa Show Supplier Material materials with Biegemodul of 25.4 GPa | ISO 178 |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 29.2 GPa Show Supplier Material materials with Elastizitätsmodul of 29.2 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 97.3 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 97.3 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 860 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 860 J/m | ASTM D 4812 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8.1 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8.1 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 9.9 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 9.9 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 55.6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 55.6 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 267.5 MPa Show Supplier Material materials with Zugfestigkeit of 267.5 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 1/K | ASTM E 831 | -40°C to 120°C |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3.4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3.4E-5 1/K | ASTM E 831 | -40°C to 120°C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Oil/Gas, Electronic Components, Enclosures, Heavy Vehicles, Air Cabin Interiors | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |