Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ | ASTM D 792 |
Relative Dichte | 23.0 °C | 1.26 [-] Show Supplier Material materials with Relative Dichte of 1.26 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 87 MPa Show Supplier Material materials with Biegefestigkeit of 87 MPa | ISO 178 | 2 mm/min | ||
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 5.4 % Show Supplier Material materials with Dehnung of 5.4 % | ISO 527 | break, 5 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527 | 1 mm/min | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 153 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 153 J/m | ASTM D 256 | notched, 23°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 12 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 116 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 116 kJ/m² | ISO 180/1U | 80*10*4, 23°C | ||
Zugfestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | ISO 527 | break, 5 mm/min | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 138 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 138 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 129 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.8E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 129 - 138 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 129 - 138 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102158629- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.6mm UL 94 |
Elektrisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Building Accessory | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |