Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.3 [-] Show Supplier Material materials with Relative Dichte of 1.3 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 100 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 120 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 120 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101793092- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 24 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 24 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | EV/HEV Battery | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |