Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Biegefestigkeit of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 3.4 GPa Show Supplier Material materials with Biegemodul of 3.4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3.4 GPa Show Supplier Material materials with Elastizitätsmodul of 3.4 GPa | ASTM D 638 | 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 26 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 165 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 165 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.86E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.86E-5 1/K | ASTM E 831 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 181 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 181 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 165 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 165 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.86E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.86E-5 1/K | ASTM E 831 | -40°C to 40°C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Food Container, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 295 to 325.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |