Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.02 [-] Show Supplier Material materials with Relative Dichte of 1.02 [-] | ASTM D 792 |
Thermisch
Property | Value | Comment |
---|---|---|
Glasübergangstemperatur | 140 °C Show Supplier Material materials with Glasübergangstemperatur of 140 °C | SABIC method | (half width) |
Elektrisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Viskosität | 23.0 °C | 0.3 Pa·s Show Supplier Material materials with Viskosität of 0.3 Pa·s | SABIC method | 50 wt% in toluene, 25°C, |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Board, Composite, Additive Plastic, Circuit Protection, Amusement Machine, Electronic Components, Fused Deposition Modeling (FDM), Electronic Material, EV Infrastructure, LED Lighting, Wire & cable, Adhesives | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |