Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.03 [-] Show Supplier Material materials with Relative Dichte of 1.03 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.8 GPa Show Supplier Material materials with Biegemodul of 0.8 GPa | ISO 178 |
Dehnung | 23.0 °C | 20 % Show Supplier Material materials with Dehnung of 20 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | ISO 527 | 1 mm/min |
Härte, Shore D | 23.0 °C | 63 [-] Show Supplier Material materials with Härte, Shore D of 63 [-] | ASTM D 2240 | 10S reading |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 37 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 25 MPa Show Supplier Material materials with Zugfestigkeit of 25 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 82 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 66 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 66 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Wärmeformbeständigkeitstemperatur | 66 - 82 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 66 - 82 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.47 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.47 [-] | ASTM D 150 |
Dissipation factor, 1GHz | 23.0 °C | 3.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 3.2E-3 [-] | ASTM D 150 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 33 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 33 g/10min | ASTM D 1238 | 280°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag, Auto Electrical, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Water Bath Temperature: 15 to 30.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |