Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.26 [-] Show Supplier Material materials with Relative Dichte of 1.26 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 107 MPa Show Supplier Material materials with Biegefestigkeit of 107 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 3.1 GPa Show Supplier Material materials with Biegemodul of 3.1 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 10 % Show Supplier Material materials with Dehnung of 10 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 214 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 214 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 214 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 214 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 66 MPa Show Supplier Material materials with Zugfestigkeit of 66 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 34 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 34 g/10min | ASTM D 1238 | 295°C/6.6 kgf | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Wireless Communications | |
Availability | Asia,Americas | |
Processing methods | Shot to Cylinder Size: 50 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |