Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.38 - 0.47 [-] Show Supplier Material materials with Coefficient of friction of 0.38 - 0.47 [-] | ||
Coefficient of friction, kinetic | 0.47 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.47 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.38 [-] Show Supplier Material materials with Coefficient of friction, static of 0.38 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.71 g/cm³ Show Supplier Material materials with Dichte of 1.71 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 227 MPa Show Supplier Material materials with Biegefestigkeit of 227 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 12.8 GPa Show Supplier Material materials with Biegemodul of 12.8 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 13.7 GPa Show Supplier Material materials with Elastizitätsmodul of 13.7 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 461 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 461 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 162 MPa Show Supplier Material materials with Zugfestigkeit of 162 MPa | ASTM D 638 | break |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 273 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 273 °C | ASTM D 648 | 3.2mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 273 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 273 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093683- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |