Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.17 g/cm³ Show Supplier Material materials with Dichte of 2.17 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Relative Dichte | 23.0 °C | 2.17 [-] Show Supplier Material materials with Relative Dichte of 2.17 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 19 MPa Show Supplier Material materials with Biegefestigkeit of 19 MPa | ISO 178 |
Biegemodul | 23.0 °C | 0.9 GPa Show Supplier Material materials with Biegemodul of 0.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 6.1 % Show Supplier Material materials with Dehnung of 6.1 % | ISO 527 | yield, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 0.9 GPa Show Supplier Material materials with Elastizitätsmodul of 0.9 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 683 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 683 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 981 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 981 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 31 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 31 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 84 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 84 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 14 MPa Show Supplier Material materials with Zugfestigkeit of 14 MPa | ISO 527 | yield, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 80 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 80 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 61 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 61 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Wärmeformbeständigkeitstemperatur | 61 - 80 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 61 - 80 °C | ||
Entflammbarkeit | UL Compliant, 94V-0 Flame Class Rating: 1.5mm UL 94 by SABIC-IP |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |