Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.61 g/cm³ Show Supplier Material materials with Dichte of 1.61 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 96 MPa Show Supplier Material materials with Biegefestigkeit of 96 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 14.3 GPa Show Supplier Material materials with Biegemodul of 14.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 0.8 % Show Supplier Material materials with Dehnung of 0.8 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 14 GPa Show Supplier Material materials with Elastizitätsmodul of 14 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 73 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 73 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 6 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 73 MPa Show Supplier Material materials with Zugfestigkeit of 73 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | ISO 11359-2 | -30°C to 80°C | ||
Thermal conductivity, through-plane | 23.0 °C | 1.5 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 1.5 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
Wärmeformbeständigkeitstemperatur | 201 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 201 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 18 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 18 W/(m·K) | ISO 22007-2 | 60*60*3mm plaque | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.77E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.77E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | Glow Wire Flammability Index 650°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 850°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1.6mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1.6mm IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.05E+6 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.05E+6 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting | |
Availability | Europe,Asia | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |