Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.24 [-] Show Supplier Material materials with Relative Dichte of 1.24 [-] | ASTM D 792 | |
Wasserabsorption | 23.0 °C | 0.12 % Show Supplier Material materials with Wasserabsorption of 0.12 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 86 MPa Show Supplier Material materials with Biegefestigkeit of 86 MPa | ISO 178 | yield, 2 mm/min | ||
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ISO 527 | yield, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ISO 527 | 1 mm/min | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 450 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 450 J/m | ASTM D 256 | -50°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 50 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 50 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Zugfestigkeit | 23.0 °C | 58 MPa Show Supplier Material materials with Zugfestigkeit of 58 MPa | ISO 527 | break, 50 mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||||
Schlagzähigkeit, Izod ungekerbt | ISO 180/1U | unnotched 80*10*3, -30°C |
Thermisch
Property | Value | Comment |
---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C |
Heat deflection temperature, 0.45 MPa | 139 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 139 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm |
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Vicat-Erweichungstemperatur | 147 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 147 °C | ISO 306 | Rate B/120 |
Wärmeformbeständigkeitstemperatur | 126 - 139 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 126 - 139 °C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 8 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 8 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung, diagonal of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components, Rail Cabin Interiors, Non-LED Lighting, Electronic Components, Air Conditioning | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |