Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Dichte of 1.19 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 122 % Show Supplier Material materials with Dehnung of 122 % | ASTM D 638 | brk, Type I, 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Supplier Material materials with Hardness, Rockwell R of 122 [-] | ASTM D 785 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 640 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 640 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Wärmeleitfähigkeit | 23.0 °C | 0.21 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.21 W/(m·K) | ASTM C177 |
Elektrisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Delivery, Respiratory, Surgical Devices, Surgical Tray | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time (Cumulative): 48hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |