Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.32 g/cm³ Show Supplier Material materials with Dichte of 1.32 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 1.09 % Show Supplier Material materials with Moisture absorption of 1.09 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Vicat-Erweichungstemperatur | 220 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 220 °C | ISO 306 | Rate B/50 | |||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236571- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Non-LED Lighting, Personal Care, Medical Device, Meter Water, Interior Rail Components, Pump, Power Boat, Pallet, Recreational Vehicle, Plumbing, Photovoltaic Components, Power Manangement, Sensor, Small Appliance, Respiratory, Washing Machine, Underhood, Tray, Swimming Pool/Spa, Wireless Communications, Weaving Machine, Water Treatment/Filtration, Weapon, Wiring Devices, Electronic Components, Energy Management, Electronics, Enclosures, Heavy Vehicles, Gas/Electric Oven, Food Processor, Fixture Bath/Shower, Engine Cooling System, Electrical, Engine Component, Auto Aftermarket, Auto Electrical, Building Accessory, Circuit Protection, Air Cabin Interiors, Defense Vehicles, Displays, Cooking Range, Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 2 to 3.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |