Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 296 MPa Show Supplier Material materials with Biegefestigkeit of 296 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 14.4 GPa Show Supplier Material materials with Biegemodul of 14.4 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 14.9 GPa Show Supplier Material materials with Elastizitätsmodul of 14.9 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 85 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 85 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 807 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 807 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 85 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 171 MPa Show Supplier Material materials with Zugfestigkeit of 171 MPa | ASTM D 638 | break |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |