Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.58 [-] Show Supplier Material materials with Coefficient of friction of 0.58 [-] | ||
Coefficient of friction, kinetic | 0.58 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.58 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.51 g/cm³ Show Supplier Material materials with Dichte of 1.51 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 211 MPa Show Supplier Material materials with Biegefestigkeit of 211 MPa | ISO 178 |
Biegemodul | 23.0 °C | 9.7 GPa Show Supplier Material materials with Biegemodul of 9.7 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | ISO 527 | break |
Zugfestigkeit | 23.0 °C | 138 MPa Show Supplier Material materials with Zugfestigkeit of 138 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.78E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.78E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.5E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282824- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Document Handling, ATM/Ticket Machine, Circuit Protection, Auto Electrical, Air Intake System, Air Filtration, Lawn/Garden, Enclosures, Electronic Components, Wiring Devices, Wireless Communications, Vacuum Cleaner, Personal Computing, Surgical Devices | |
Availability | Asia,Americas | |
Processing methods | Back Pressure: 0.2 to 0.3MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |