Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.03 [-] Show Supplier Material materials with Relative Dichte of 1.03 [-] | ASTM D 792 |
Sauerstoffindex | 23.0 °C | 25 % Show Supplier Material materials with Sauerstoffindex of 25 % | |
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | ASTM D 570 | (23°C/48hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.7 GPa Show Supplier Material materials with Biegemodul of 0.7 GPa | ISO 178 | 12.5 mm/min |
Dehnung | 23.0 °C | 90 % Show Supplier Material materials with Dehnung of 90 % | ISO 527 | break, 50 mm/min |
Härte, Shore D | 23.0 °C | 56 [-] Show Supplier Material materials with Härte, Shore D of 56 [-] | ISO 868 |
Zugfestigkeit | 23.0 °C | 23 MPa Show Supplier Material materials with Zugfestigkeit of 23 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Heat deflection temperature, 0.45 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ASTM D 648 | 6.4 mm, unannealed | |
Vicat-Erweichungstemperatur | 102 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 102 °C | ISO 306 | Rate A/50 | |
Wärmeformbeständigkeitstemperatur | 85 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 85 °C | ||
Entflammbarkeit | Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 75- ASTM E 662 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Smoke Density on 0.5mm plaque, Flame, Ds, max: 150- ASTM E 662 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.6 [-] | IEC 60250 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.5 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.5 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 3.8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.8E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 0.02 [-] | IEC 60250 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 26 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 26 kV/mm | IEC 60243-1 | in oil, 2.0mm |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 | |
Volume resistivity | 23.0 °C | 3.90E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.90E+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 5.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 5.1 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer, Wire & cable | |
Availability | Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |