Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 226 MPa Show Supplier Material materials with Biegefestigkeit of 226 MPa | ISO 178 |
Biegemodul | 23.0 °C | 16.5 GPa Show Supplier Material materials with Biegemodul of 16.5 GPa | ISO 178 |
Dehnung | 23.0 °C | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 16.7 GPa Show Supplier Material materials with Elastizitätsmodul of 16.7 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 480 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 480 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 9 J Show Supplier Material materials with Instrumented Impact, at Peak of 9 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 32 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 148 MPa Show Supplier Material materials with Zugfestigkeit of 148 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 143 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.71E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.71E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 140 - 143 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 140 - 143 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 2.78E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 2.78E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283808- - <br> UL Recognized, 94V-1 Flame Class Rating: 1.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |