Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.01 [-] Show Supplier Material materials with Relative Dichte of 1.01 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.1 GPa Show Supplier Material materials with Biegemodul of 0.1 GPa | ISO 178 | 12.5 mm/min |
Dehnung | 23.0 °C | 175 % Show Supplier Material materials with Dehnung of 175 % | ISO 527 | break, 50 mm/min |
Härte, Shore A | 23.0 °C | 84 [-] Show Supplier Material materials with Härte, Shore A of 84 [-] | ASTM D 2240 | 30S reading |
Zugfestigkeit | 23.0 °C | 7 MPa Show Supplier Material materials with Zugfestigkeit of 7 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101939210- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> Glow Wire Flammability Index 750°C, passes at: 3mm IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 0 V Show Supplier Material materials with Kriechstromfestigkeit of 0 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 7.10E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 7.10E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 24 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 24 g/10min | ASTM D 1238 | 210°C/5 kgf | |
Schrumpfung | 23.0 °C | 0.95 % Show Supplier Material materials with Schrumpfung of 0.95 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.75 % Show Supplier Material materials with Schrumpfung, diagonal of 0.75 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 60 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |