Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.16 [-] Show Supplier Material materials with Relative Dichte of 1.16 [-] | ASTM D 792 |
Sauerstoffindex | 23.0 °C | 33.9 % Show Supplier Material materials with Sauerstoffindex of 33.9 % | |
Wasserabsorption | 23.0 °C | 0.07 % Show Supplier Material materials with Wasserabsorption of 0.07 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 119 MPa Show Supplier Material materials with Biegefestigkeit of 119 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 4 GPa Show Supplier Material materials with Biegemodul of 4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 96 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 96 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 74 MPa Show Supplier Material materials with Zugfestigkeit of 74 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 131 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Vicat-Erweichungstemperatur | 147 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 147 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 131 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 131 °C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221214- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100072184- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3 [-] | ASTM D 150 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 1.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1.6E-3 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 1.7E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1.7E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Auto Electrical, Battery Pack, Audio, Auto Aftermarket, Aerospace, Coffee Maker/Espresso Machine, Cladding/Roof, Document Handling, Displays, Dishwasher, Enclosures, Enclosure/Housing/Cover, Energy Management, Electronic Components, Humidity Control, Individual Equiptment, Eyeglasses, Freezer, Fixture Bath/Shower, Engine Component, EV/HEV Battery, Wiring Devices, Wireless Communications, Personal Computing, Monitoring and Imaging, Meter Gas, Medical Device, Respiratory, Plumbing, Photovoltaic Components, Power Manangement, Pump | |
Availability | Europe,Asia,Americas | |
Processing methods | Shot to Cylinder Size: 30 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |