Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 99 MPa Show Supplier Material materials with Biegefestigkeit of 99 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 4.3 % Show Supplier Material materials with Dehnung of 4.3 % | ISO 527 | yield, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 180 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 180 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 14 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 61 MPa Show Supplier Material materials with Zugfestigkeit of 61 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 3.0 mm | |
Heat deflection temperature, 0.45 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 129 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 115 - 129 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 115 - 129 °C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> Radiant Panel Listing: RP100- UL Tested <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Flammability Index, 1.0 mm: 900°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 900°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 700°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 700°C IEC 60695-2-13 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100107147- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100107136- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.52 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.52 [-] | ASTM D 150 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.46 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.46 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 2.1E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.1E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.4E-3 [-] | ASTM D 150 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 18.1 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 18.1 kV/mm | ASTM D 149 | in oil, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 1 V Show Supplier Material materials with Kriechstromfestigkeit of 1 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 2.30E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.30E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning, Aerospace, Circuit Protection, Auto Electrical, ATM/Ticket Machine, Auto Aftermarket, Displays, Document Handling, Building Element, Data Transfer, Data Management, Electronic Components, Enclosure/Housing/Cover, Electronics, Energy Management, Enclosures, Lab Ware and Clinical Diagnostics, Lawn/Garden, Hot Water System, Head Protection, Gear/Bearing/Slider, Fixture Bath/Shower, Food Processor, Electronic Material Handling, Wiring Devices, Wireless Communications, Washing Machine, Vending Machine, Personal Computing, Non-LED Lighting, Medical Device, LED Lighting, Microwave Oven, Laundry Dryer, Monitoring and Imaging, Small Appliance, Surgical Devices, Safety Glasses, Security/Detection, Refrigerator, Pump, Photovoltaic Components, Power Manangement | |
Availability | Asia,Americas | |
Processing methods | Drying Time: 3 to 4.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |