Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative Dichte of 1.25 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 117 MPa Show Supplier Material materials with Biegefestigkeit of 117 MPa | ISO 178 |
Biegemodul | 23.0 °C | 3.8 GPa Show Supplier Material materials with Biegemodul of 3.8 GPa | ISO 178 |
Dehnung | 23.0 °C | 3.7 % Show Supplier Material materials with Dehnung of 3.7 % | ISO 527 | yield |
Elastizitätsmodul | 23.0 °C | 4 GPa Show Supplier Material materials with Elastizitätsmodul of 4 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 131 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 131 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2230 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2230 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 443 J Show Supplier Material materials with Instrumented Impact, Total Energy of 443 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO 179/2C | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 9 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 57 MPa Show Supplier Material materials with Zugfestigkeit of 57 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 126 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 111 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.06E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.06E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 100 °C Show Supplier Material materials with Relative temperature index, electrical of 100 °C | UL 746B | |||
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |||
Relative temperature index, mechanical strength | 100 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 100 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 132 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 132 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 111 - 126 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 111 - 126 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.76E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.76E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Radiant Panel Listing: TRUE- UL Tested <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221170- - <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.89 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.89 [-] | ASTM D 150 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.7 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 4.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 4.4E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 0.02 [-] | ASTM D 150 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 17.3 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 17.3 kV/mm | ASTM D 149 | in oil, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.20E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.20E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 7.6 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 7.6 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Schmelzvolumenflussrate | 6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 6 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Laundry Dryer, Meter Gas, Personal Computing, Non-LED Lighting, Oil/Gas, Security/Detection, Respiratory, Small Appliance, Power Manangement, Wireless Communications, Wiring Devices, Wearables, Washing Machine, Building Accessory, Battery Cell, Circuit Protection, Air Conditioning, Document Handling, Displays, Dishwasher, Data Transfer, Electronic Components, Enclosure/Housing/Cover, Enclosures, Individual Equiptment, Hygiene/Personal Care, Furnace/Heater, Food Processor | |
Availability | Americas | |
Processing methods | Shot to Cylinder Size: 30 to 70.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |