Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break, 5 mm/min |
Zugfestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 135 - 140 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 135 - 140 °C | ||||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236778- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.1 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.1 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 8E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 8E-3 [-] | IEC 60250 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Cladding/Roof, Document Handling, Enclosures, Enclosure/Housing/Cover, Electronic Components, Hot Water System, Lawn/Garden, Fixture Bath/Shower, Furnace/Heater, Electronic Material Handling, Washing Machine, Wiring Devices, Wireless Communications, Motorcycle, Personal Care, Medical Device, LED Lighting, Surgical Devices, Small Appliance, Security/Detection, Renal and Blood Handling, Pump, Refrigerator | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 280 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |