Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 5.6 GPa Show Supplier Material materials with Biegemodul of 5.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | ISO 527 | break, 50 mm/min |
Zugfestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 133 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 133 - 135 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 133 - 135 °C | ||||
Entflammbarkeit | Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236777- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
High Amp Arc Ignition | 23.0 °C | 6 mm Show Supplier Material materials with High Amp Arc Ignition of 6 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Pump, Pipe/Fitting, Power Manangement, Photovoltaic Components, Plumbing, Respiratory, Security/Detection, Sensor, Surgical Devices, Meter Gas, Ignition System, Meter Water, Microwave Oven, Personal Computing, Motorcycle, Non-LED Lighting, Wireless Communications, Wiring Devices, Water Treatment/Filtration, Wearables, Washing Machine, Travel Suitcase, Traffic Management, Swimming Pool/Spa, EV/HEV Battery, Electronic Material Handling, EV Infrastructure, Fixture Bath/Shower, Individual Equiptment, Industrial Material Handling, HVAC Underhood, Hygiene/Personal Care, Lab Ware and Clinical Diagnostics, Humidity Control, Hot Water System, Heavy Vehicles, Electronic Components, Energy Management, Electronics, Enclosure/Housing/Cover, Enclosures, Dishwasher, Defense Vehicles, Drain Pan, Displays, Document Handling, Cluster, Coffee Maker/Espresso Machine, Building Element, Battery System, Data Transfer, Air Conditioning, Auto Aftermarket, Audio, ATM/Ticket Machine, Battery Pack, Building Accessory, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 260 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |