Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.11 [-] Show Supplier Material materials with Relative Dichte of 1.11 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 103 MPa Show Supplier Material materials with Biegefestigkeit of 103 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 4 J Show Supplier Material materials with Instrumented Impact, Total Energy of 4 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 74 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 74 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 185 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.1E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Vicat-Erweichungstemperatur | 197 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 197 °C | ISO 306 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 185 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.6E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1000 - 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 - 10000 Ω·cm | SABIC method |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 25 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 25 g/10min | ASTM D 1238 | 300°C/5.0 kgf | |
Schrumpfung | 23.0 °C | 1 % Show Supplier Material materials with Schrumpfung of 1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Seating/Chair | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Maximum Moisture Content: 0.07% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |