Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.15 [-] Show Supplier Material materials with Relative Dichte of 1.15 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 47 MPa Show Supplier Material materials with Biegefestigkeit of 47 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 1.5 GPa Show Supplier Material materials with Biegemodul of 1.5 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 1.8 GPa Show Supplier Material materials with Elastizitätsmodul of 1.8 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 40 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 40 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 667 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 667 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 40 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+9 - 1.00E+11 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+9 - 1.00E+11 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+9 - 1.00E+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+9 - 1.00E+11 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 70 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |