Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.26 [-] Show Supplier Material materials with Relative Dichte of 1.26 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 203 MPa Show Supplier Material materials with Biegefestigkeit of 203 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 9.3 GPa Show Supplier Material materials with Biegemodul of 9.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 10.6 GPa Show Supplier Material materials with Elastizitätsmodul of 10.6 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 88 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 88 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 591 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 591 J/m | ASTM D 4812 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | ISO 179/2C | 23°C |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | ISO 179/2C | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 88 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 88 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Wärmeformbeständigkeitstemperatur | 123 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 123 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102010749- - <br> UL Recognized, 94HB Flame Class Rating: 1mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 5000 - 500000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 5000 - 500000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 5.00E+4 - 5.00E+6 Ω·cm Show Supplier Material materials with Volume resistivity of 5.00E+4 - 5.00E+6 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 30 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 30 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung, diagonal of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |