Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.19 % Show Supplier Material materials with Moisture absorption of 0.19 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative Dichte of 1.25 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 88 MPa Show Supplier Material materials with Biegefestigkeit of 88 MPa | ISO 178 |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 16 % Show Supplier Material materials with Dehnung of 16 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 337 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 337 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 940 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 940 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 38 J Show Supplier Material materials with Instrumented Impact, Total Energy of 38 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 21 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 21 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 48 MPa Show Supplier Material materials with Zugfestigkeit of 48 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 127 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.2E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | |||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 127 - 136 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 127 - 136 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.52E-3 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.52E-3 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101212124- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1000 - 1000000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1000 - 1000000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 - 1000000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Personal Computing, Power Manangement | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |