Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 82 MPa Show Supplier Material materials with Biegefestigkeit of 82 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 13.5 % Show Supplier Material materials with Dehnung of 13.5 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1810 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1810 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 150 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 150 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 46 MPa Show Supplier Material materials with Zugfestigkeit of 46 MPa | ASTM D 638 | break |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 73 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 73 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-4 1/K | ASTM D 696 | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 73 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 73 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 2.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 2.8 W/(m·K) | ASTM E 1530 | |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |