Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Sauerstoffindex | 23.0 °C | 47 % Show Supplier Material materials with Sauerstoffindex of 47 % | |
Schüttdichte | 23.0 °C | 0.78 g/cm³ Show Supplier Material materials with Schüttdichte of 0.78 g/cm³ | ASTM D 1895 |
Wasserabsorption | 23.0 °C | 0.25 % Show Supplier Material materials with Wasserabsorption of 0.25 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 151 MPa Show Supplier Material materials with Biegefestigkeit of 151 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 3.3 GPa Show Supplier Material materials with Biegemodul of 3.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3.6 GPa Show Supplier Material materials with Elastizitätsmodul of 3.6 GPa | ASTM D 638 | 5 mm/min |
Härte, Rockwell M | 23.0 °C | 109 [-] Show Supplier Material materials with Härte, Rockwell M of 109 [-] | ASTM D 785 | |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 53 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 53 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 201 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 201 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.58E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.58E-5 1/K | ASTM E 831 | -20°C to 150°C |
Vicat-Erweichungstemperatur | 218 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 218 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 201 - 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 201 - 210 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | ASTM C177 |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.4E-5 1/K | ASTM E 831 | -20°C to 150°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 28 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 28 kV/mm | ASTM D 149 | in oil, 1.6 mm |
Verlustfaktor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Verlustfaktor of 2.5E-3 [-] | ASTM D 150 | 2450 MHz |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Composite | |
Availability | Europe,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |