Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Dichte of 1.46 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.27 % Show Supplier Material materials with Moisture absorption of 0.27 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.46 [-] Show Supplier Material materials with Relative Dichte of 1.46 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 155 MPa Show Supplier Material materials with Biegefestigkeit of 155 MPa | ISO 178 |
Biegemodul | 23.0 °C | 4.3 GPa Show Supplier Material materials with Biegemodul of 4.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 4.3 % Show Supplier Material materials with Dehnung of 4.3 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 4.3 GPa Show Supplier Material materials with Elastizitätsmodul of 4.3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 34 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 34 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 485 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 485 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 33 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Zugfestigkeit of 98 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 194 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 194 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 177 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 177 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4E-5 1/K | ASTM D 696 | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 177 - 194 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 177 - 194 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4.4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4.4E-5 1/K | ASTM D 696 | -30°C to 30°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000 Ω | ASTM D 257 |
Shielding effectiveness | 23.0 °C | 60 dB Show Supplier Material materials with Shielding effectiveness of 60 dB | SABIC method | @ 2.5mm |
Volume resistivity | 23.0 °C | 89 Ω·cm Show Supplier Material materials with Volume resistivity of 89 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Data Transfer | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |