Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.52 - 0.55 [-] Show Supplier Material materials with Coefficient of friction of 0.52 - 0.55 [-] | ||
Coefficient of friction, kinetic | 0.55 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.55 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.52 [-] Show Supplier Material materials with Coefficient of friction, static of 0.52 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Dichte of 1.3 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 152 MPa Show Supplier Material materials with Biegefestigkeit of 152 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 5.7 GPa Show Supplier Material materials with Biegemodul of 5.7 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 8.2 GPa Show Supplier Material materials with Elastizitätsmodul of 8.2 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 74 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 74 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 283 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 283 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 13 J Show Supplier Material materials with Instrumented Impact, at Peak of 13 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 34 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 34 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 101 MPa Show Supplier Material materials with Zugfestigkeit of 101 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 143 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Wärmeformbeständigkeitstemperatur | 143 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 143 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.6E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 100 Ω·cm Show Supplier Material materials with Volume resistivity of 100 Ω·cm | IEC 60093 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |