Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 160 MPa Show Supplier Material materials with Biegefestigkeit of 160 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 3.3 GPa Show Supplier Material materials with Biegemodul of 3.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | SABIC method | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 211 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 211 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 190 - 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 - 200 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.21 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.21 W/(m·K) | ISO 8302 | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101048269- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 16 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Verlustfaktor | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Verlustfaktor of 2.5E-3 [-] | IEC 60250 | 2450 MHz |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Tray, Surgical Tray, Sunglasses, Wiring Devices, Wearables, Water Treatment/Filtration, Wireless Communications, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Pharmaceutical Packaging & Drug Delivery, Power Manangement, Photovoltaic Components, Respiratory, Safety Glasses, Semiconductor, Security/Detection, Surgical Devices, Small Appliance, Smart/ID Card, Ignition System, Interior Rail Components, Meter Gas, Monitoring and Imaging, Medical Device, LED Lighting, Personal Computing, Oil/Gas, Personal Care, OLED, Lighting, Non-LED Lighting, Enclosure/Housing/Cover, Electronics, Enclosures, Electronic Components, Lab Ware and Clinical Diagnostics, Individual Equiptment, Industrial Material Handling, Fuel Cell, Gas/Electric Oven, Humidity Control, Eyeglasses, Front Grille, Forward Lighting, Food Processor, Food Container, Fog Lamp, Fluid Delivery, Exterior Rail Components, Electronic Material Handling, Engine Cooling System, Exterior Trim, Air Cabin Interiors, Aircraft Seating, Aerospace, Auto Electrical, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, Composite, Commercial Storage/Cookware, Cooking Range, Coffee Maker/Espresso Machine, Data Transfer, Data Management, Displays, Dishwasher, Document Handling, Wire & cable, Adhesives | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |