Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Dichte of 1.47 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 267 MPa Show Supplier Material materials with Biegefestigkeit of 267 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 16.3 GPa Show Supplier Material materials with Biegemodul of 16.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 3.7 % Show Supplier Material materials with Dehnung of 3.7 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 13.5 GPa Show Supplier Material materials with Elastizitätsmodul of 13.5 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 9 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 35 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 201 MPa Show Supplier Material materials with Zugfestigkeit of 201 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 220 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 220 °C | UL 746B | |
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284426- - <br> UL Recognized, 94V-0 Flame Class Rating: 0.7mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |