Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.91 % Show Supplier Material materials with Moisture absorption of 0.91 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 241 MPa Show Supplier Material materials with Biegefestigkeit of 241 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 11.7 GPa Show Supplier Material materials with Elastizitätsmodul of 11.7 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 907 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 907 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 106 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 106 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 159 MPa Show Supplier Material materials with Zugfestigkeit of 159 MPa | ASTM D 638 | break |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Electronic Components, Power Manangement | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |