Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 83 MPa Show Supplier Material materials with Biegefestigkeit of 83 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 75 % Show Supplier Material materials with Dehnung of 75 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 181 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 181 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, at Peak | 23.0 °C | 38 J Show Supplier Material materials with Instrumented Impact, at Peak of 38 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 181 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 181 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 126 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 126 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221026- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=228457- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Optisch
Property | Value | Comment |
---|---|---|
Gloss | 52 [-] Show Supplier Material materials with Gloss of 52 [-] | ASTM D 523 | untextured, 60 degrees |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 21.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 21.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Document Handling, Displays, Personal Computing, LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |