Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 90 MPa Show Supplier Material materials with Biegefestigkeit of 90 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Biegemodul of 2.1 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 100 % Show Supplier Material materials with Dehnung of 100 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 600 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 600 J/m | ASTM D 256 | -40°C |
Instrumented Impact, Total Energy | 23.0 °C | 70 J Show Supplier Material materials with Instrumented Impact, Total Energy of 70 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 800 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 800 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 1.80 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 145 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 145 °C | ASTM D 1525 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 123 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 123 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 875°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 850°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 850°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100651927- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 9.3E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 9.3E-3 [-] | ASTM D 150 |
Durchschlagfestigkeit | 23.0 °C | 15 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15 kV/mm | ASTM D 149 | in oil, 0.8 mm |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 3 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 10 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Heavy Vehicles, Data Transfer, Audio | |
Availability | Europe,Asia | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |