Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 107 MPa Show Supplier Material materials with Biegefestigkeit of 107 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 3.2 % Show Supplier Material materials with Dehnung of 3.2 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 213 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 213 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 31 J Show Supplier Material materials with Instrumented Impact, Total Energy of 31 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 10 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 61 MPa Show Supplier Material materials with Zugfestigkeit of 61 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 95 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.74E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.74E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 108 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 108 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 82 - 95 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 82 - 95 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: 0.99mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: 1.49mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2.99mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 2 mm Show Supplier Material materials with High Amp Arc Ignition of 2 mm | UL 746A | surface {PLC} |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 2 mm Show Supplier Material materials with Hot-Wire Ignition of 2 mm | UL 746A | (PLC) |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 14 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 14 g/10min | ASTM D 1238 | 220°C/2.16 kgf | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 75 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |