Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 3.5 % Show Supplier Material materials with Wasserabsorption of 3.5 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Biegefestigkeit of 70 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 8 % Show Supplier Material materials with Dehnung of 8 % | ISO 527 | yield, 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 13 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 15 mg/1000cy Show Supplier Material materials with Taber Abrasion of 15 mg/1000cy | SABIC method | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Vicat-Erweichungstemperatur | 166 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 166 °C | ISO 306 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 154 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 154 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Wheel Cover, Recreational Vehicle, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |