Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Biegefestigkeit of 98 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 117 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 117 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 117 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 63 MPa Show Supplier Material materials with Zugfestigkeit of 63 MPa | SABIC - Japan Method | yield |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | TMA | -30°C to 30°C | ||
Wärmeformbeständigkeitstemperatur | 105 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 105 °C | ||||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.78 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.78 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3E-3 [-] | ASTM D 150 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 17 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17 g/10min | ASTM D 1238 | 250°C/10.0 kgf | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic Components, Power Manangement, Personal Computing, Washing Machine, Wireless Communications, Document Handling, Displays, Battery Cell, Battery Pack, Auto Electrical, EV Infrastructure, EV/HEV Battery, Enclosures, Energy Management, Enclosure/Housing/Cover, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 75 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |