NORYL™ N1050 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade was designed for improved dimensional stability and flow. This grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 1.5mm along with impact strength, very low moisture absorption, excellent dimensional stability, and good electrical properties. NORYL N1050 resin is an excellent candidate for a variety of applications requiring electrically insulating properties, low moisture absorption and low warpage.

Diese Materialdaten wurden von Sabic zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Relative Dichte

23.0 °C

1.1 [-]

Show Supplier Material materials with Relative Dichte of 1.1 [-]

ASTM D 792 |

Wasserabsorption

23.0 °C

0.07 %

Show Supplier Material materials with Wasserabsorption of 0.07 %

ASTM D 570 | (23°C/24hrs)

Mechanisch

PropertyTemperatureValueComment

Biegefestigkeit

23.0 °C

98 MPa

Show Supplier Material materials with Biegefestigkeit of 98 MPa

ASTM D 790

Biegemodul

23.0 °C

2.5 GPa

Show Supplier Material materials with Biegemodul of 2.5 GPa

ASTM D 790

Dehnung

23.0 °C

40 %

Show Supplier Material materials with Dehnung of 40 %

SABIC - Japan Method | break

Impact strength, Izod notched, ASTM

23.0 °C

117 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m

ASTM D 256 | notched, 23°C

Schlagzähigkeit, Izod gekerbt

23.0 °C

117 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 117 kJ/m²

ASTM D 256 | notched, 23°C

Zugfestigkeit

23.0 °C

63 MPa

Show Supplier Material materials with Zugfestigkeit of 63 MPa

SABIC - Japan Method | yield

Thermisch

PropertyTemperatureValueComment

Heat deflection temperature, 1.80 MPa

105 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C

ASTM D 648 | 6.4 mm, unannealed

Koeffizient der thermischen Ausdehnung

23.0 °C

7E-5 1/K

Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K

TMA | -30°C to 30°C

Wärmeformbeständigkeitstemperatur

105 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 105 °C

Entflammbarkeit

UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2.5mm UL 94

Elektrisch

PropertyTemperatureValueComment

Dielectric constant, 60Hz

23.0 °C

2.78 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.78 [-]

ASTM D 150 | 50/60 Hz

Dissipation factor, 50Hz

23.0 °C

3E-3 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 3E-3 [-]

ASTM D 150 | 50/60 Hz

Sheet resistivity, ROA

23.0 °C

1.00E+16 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Schmelzmassenflussrate

17 g/10min

Show Supplier Material materials with Schmelzmassenflussrate of 17 g/10min

ASTM D 1238 | 250°C/10.0 kgf

Schrumpfung

23.0 °C

0.5 %

Show Supplier Material materials with Schrumpfung of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Photovoltaic Components, Power Manangement, Personal Computing, Washing Machine, Wireless Communications, Document Handling, Displays, Battery Cell, Battery Pack, Auto Electrical, EV Infrastructure, EV/HEV Battery, Enclosures, Energy Management, Enclosure/Housing/Cover, Electronic Components

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 75 to 80.0°C
Drying Time: 3 to 4.0hrs
Drying Time (Cumulative): 8hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 250 to 275.0°C
Nozzle Temperature: 250 to 275.0°C
Front - Zone 3 Temperature: 240 to 275.0°C
Middle - Zone 2 Temperature: 225 to 270.0°C
Rear - Zone 1 Temperature: 215 to 265.0°C
Mold Temperature: 55 to 75.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 20 to 100.0rpm
Shot to Cylinder Size: 30 to 70.0%
Vent Depth: 0.038 to 0.051mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.