Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.21 [-] Show Supplier Material materials with Coefficient of friction of 0.21 [-] | ||
Coefficient of friction, kinetic | 0.21 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.21 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.07 g/cm³ Show Supplier Material materials with Dichte of 1.07 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 91 MPa Show Supplier Material materials with Biegefestigkeit of 91 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 11.9 % Show Supplier Material materials with Dehnung of 11.9 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | ASTM D 638 | 50 mm/min |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Supplier Material materials with Hardness, Rockwell R of 115 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 230 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 230 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 230 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 230 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.2E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.2E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 124 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 124 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.6E-4 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.6E-4 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284063- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=102991929- - <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 38 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 38 cm³/10min | ISO 1133 | MVR at 280°C/10.0 kg | |
Schrumpfung | 23.0 °C | 0.94 % Show Supplier Material materials with Schrumpfung of 0.94 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.91 % Show Supplier Material materials with Schrumpfung, diagonal of 0.91 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |