Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.5 % Show Supplier Material materials with Wasserabsorption of 0.5 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 12 MPa Show Supplier Material materials with Biegefestigkeit of 12 MPa | ISO 178 |
Biegemodul | 23.0 °C | 0.3 GPa Show Supplier Material materials with Biegemodul of 0.3 GPa | ISO 178 |
Dehnung | 23.0 °C | 90 % Show Supplier Material materials with Dehnung of 90 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 0.3 GPa Show Supplier Material materials with Elastizitätsmodul of 0.3 GPa | ISO 527 | 1 mm/min |
Härte, Shore D | 23.0 °C | 56 [-] Show Supplier Material materials with Härte, Shore D of 56 [-] | ASTM D 2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 580 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 580 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 150 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 150 kJ/m² | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 23 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 23 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 22 MPa Show Supplier Material materials with Zugfestigkeit of 22 MPa | ASTM D 638 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 88 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 88 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 57 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 57 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-4 1/K | ISO 11359-2 | -40°C to 40°C | ||
Wärmeformbeständigkeitstemperatur | 57 - 88 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 57 - 88 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.8E-4 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.8E-4 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093722- - <br> UL Recognized, 94HB Flame Class Rating: 1mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Document Handling, Lawn/Garden | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |