Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.15 [-] Show Supplier Material materials with Relative Dichte of 1.15 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 103 MPa Show Supplier Material materials with Biegefestigkeit of 103 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 6.9 GPa Show Supplier Material materials with Biegemodul of 6.9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Supplier Material materials with Hardness, Rockwell R of 122 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 240 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 240 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 83 mg/1000cy Show Supplier Material materials with Taber Abrasion of 83 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 71 MPa Show Supplier Material materials with Zugfestigkeit of 71 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 111 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 105 - 111 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 105 - 111 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221166- - <br> UL Recognized, 94V-1 Flame Class Rating: 2mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2mm UL 94 |
Elektrisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical Components & Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |