Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 135 MPa Show Supplier Material materials with Biegefestigkeit of 135 MPa | ISO 178 | yield, 2 mm/min |
Dehnung | 23.0 °C | 8 % Show Supplier Material materials with Dehnung of 8 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 4.5 GPa Show Supplier Material materials with Elastizitätsmodul of 4.5 GPa | ISO 527 | 1 mm/min |
Zugfestigkeit | 23.0 °C | 75 MPa Show Supplier Material materials with Zugfestigkeit of 75 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 189 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 189 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 189 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 189 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥0.41mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221097- - <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Technological properties
Property | ||
---|---|---|
Application areas | Respiratory, Monitoring and Imaging, Air Cabin Interiors, Electronic Components, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Middle - Zone 2 Temperature: 360 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |