Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 154 MPa Show Supplier Material materials with Biegefestigkeit of 154 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 10.3 GPa Show Supplier Material materials with Biegemodul of 10.3 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 4 - 6 % Show Supplier Material materials with Dehnung of 4 - 6 % | SABIC - Japan Method | break |
Härte, Rockwell M | 23.0 °C | 90 [-] Show Supplier Material materials with Härte, Rockwell M of 90 [-] | ASTM D 785 | |
Impact strength, Izod notched, ASTM | 23.0 °C | 68 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 68 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 68 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 68 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 116 MPa Show Supplier Material materials with Zugfestigkeit of 116 MPa | SABIC - Japan Method | yield |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 - 3.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 - 3.3E-5 1/K | TMA | -30°C to 30°C | ||
Wärmeformbeständigkeitstemperatur | 125 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 °C | ||||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228551- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 15.4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15.4 g/10min | ASTM D 1238 | 300°C/2.16 kgf | |
Schrumpfung | 23.0 °C | 0.15 % Show Supplier Material materials with Schrumpfung of 0.15 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Small Appliance, Power Manangement, Wireless Communications, Building Accessory, Document Handling, Displays, Electronic Components, Enclosures | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Back Pressure: 0.3 to 0.7MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |