Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.35 % Show Supplier Material materials with Wasserabsorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 90 MPa Show Supplier Material materials with Biegefestigkeit of 90 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 220 % Show Supplier Material materials with Dehnung of 220 % | SABIC - Japan Method | break |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 65 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Zugfestigkeit | 23.0 °C | 61 MPa Show Supplier Material materials with Zugfestigkeit of 61 MPa | SABIC - Japan Method | yield |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | TMA | -30°C to 30°C |
Wärmeformbeständigkeitstemperatur | 133 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 133 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Audio, Auto Aftermarket, Data Transfer, Data Management, Cluster, Console, Displays, Doors Hardware/Trim, Forward Lighting, Heavy Vehicles, Infotainment/Telematic, Electronic Components, Power Manangement, Rear/Signal Lighting, Small Appliance, Surgical Devices, Non-LED Lighting, Personal Computing, Meter Gas, LED Lighting, Wireless Communications, Trim | |
Availability | Europe,Asia | |
Processing methods | Front - Zone 3 Temperature: 280 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |