Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.34 - 0.42 [-] Show Supplier Material materials with Coefficient of friction of 0.34 - 0.42 [-] | ||
Coefficient of friction, kinetic | 0.42 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.42 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.34 [-] Show Supplier Material materials with Coefficient of friction, static of 0.34 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 146 MPa Show Supplier Material materials with Biegefestigkeit of 146 MPa | ISO 178 |
Biegemodul | 23.0 °C | 5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | ISO 178 |
Dehnung | 23.0 °C | 3.4 % Show Supplier Material materials with Dehnung of 3.4 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 7.2 GPa Show Supplier Material materials with Elastizitätsmodul of 7.2 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 501 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 501 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 15 J Show Supplier Material materials with Instrumented Impact, at Peak of 15 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 11 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 40 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Zugfestigkeit of 98 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 138 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 138 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.02E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.02E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Wärmeformbeständigkeitstemperatur | 138 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 138 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.18E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.18E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344536- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343859- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |