Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.32 [-] Show Supplier Material materials with Relative Dichte of 1.32 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 260 MPa Show Supplier Material materials with Biegefestigkeit of 260 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 18 GPa Show Supplier Material materials with Biegemodul of 18 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 21 GPa Show Supplier Material materials with Elastizitätsmodul of 21 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 70 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 70 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 500 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 500 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 10 J Show Supplier Material materials with Instrumented Impact, Total Energy of 10 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 70 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 185 MPa Show Supplier Material materials with Zugfestigkeit of 185 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 86 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 86 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 86 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 86 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 3.5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 3.5E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101712652- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.7mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.40E+6 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.40E+6 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 3.19E+6 Ω·cm Show Supplier Material materials with Volume resistivity of 3.19E+6 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 70°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |